Abstract:The rotating groove in shell of one spent fuel transfer tank was cracked in the manufacture process. To determine the failure cause and prevent the similar failure event happening again, the chemical composition, mechanical properties, metallographic structure, and fracture morphology were analyzed to find out the fracture causes. The results showed that the failure model of the rotating groove was hydrogen-induced delayed cracking. The high content of hydrogen and aging embrittlement were the main reasons to cause hydrogen induced cracking of rotating groove.
[1] 叶国安,郑卫芳,何辉,等.我国核燃料后处理技术现状和发展[J].原子能科学技术,2020,54(S1):75-83. YE Guoan,ZHENG Weifang,HE Hui,et al.Statue and development of technology on reprocessing spent nuclear fuel in China[J].Atomic Energy Science and Technology,2020,54(S1):75-83. [2] Zhang T Y, Chu W Y,Hsiao C M.Tetragonal distortion field of hydrogen atoms in iron[J].Metallurgical Transactions A, 1985,16(9):1649-53. [3] Wang M Q,Akiyama E,Tsuzaki K.Determination of the critical hydrogen concentration for delayed fracture of high strength steel by constant load test and numerical calculation[J].Corrosion Science,2006,48(8):2189-2202. [4] 刘德林,陶春虎,刘昌奎,等.钢氢脆失效的新现象和新认识[J].失效分析与预防,2015,10(6):376-383. LIU Delin,TAO Chunhu,LIU Changkui,et al.New phenomenons and knowledge of steel hydrogen embrittlement[J].Failire Analysis and Prevention,2015,10(6):376-383. [5] 谢金鹏,林双平,钟振前,等.0Cr17Ni4Cu4Nb传感器断裂原因分析[J].冶金分析,2019,39(7):53-57. XIE Jinpeng,LIN Shuangpin,ZHONG Zhenqian,et al.Fracture cause analysis of 0Cr17Ni4Cu4 Nb sensor[J].Metallurgical Analysis,2019,39(7):53-57. [6] Sezgin J G,Yamabe J.Simulation of the impact of internal pressure on the integrity of a hydrogen-charged Type-316L stainless steel during slow strain rate tensile test[J].International Journal of Hydrogen Energy,2018,43(17):8558-8568. [7] 王剑星,杨钢,张忠模,等.热处理工艺对0Cr17Ni4Cu4Nb不锈钢组织和力学性能的影响[J].金属热处理,2012,37(11):90-94. WANG Jianxing,YANG Gang,ZHANG Zhongmo,et al.Effect of heat treatment process on microstructure and mechanical properties of 0Cr17Ni4Cu4Nb stainless steel[J].Heat Treatment of Metals,2012,37(11):90-94. [8] Thomas R L S,Scully J R,Gangloff R P. Internal hydrogen embrittlement of ultrahigh strength Aer Met 100 steel[J].Metallurgical and Materials Transactions A,2003,34(2):327-344. [9] 王富强,王磊,刘杨,等.氢对GH690合金断裂韧性和断裂行为的影响[J].腐蚀科学与防护技术,2010,22(5):380-384. WANG Fuqiang,WANG Lei,LIU Yang,et al.Effect of hydrogen on fracture toughness and fracture behavior of GH690 alloy[J].Corrosion Science and Protection Technology,2010,22(5):380-384. [10] 管真,孙永庆,李莉,等.15-5PH不锈钢的氢脆敏感性[J].金属热处理,2019,44(12):226-232. GUAN Zhen,SUN Yongqiang,LI Li,et al.Hydrogen embrittlement sensitivity of 15-5PH stainless steel[J].Heat Treatment of Metals,2019,44(12):226-232.